Ceramic and granite stone is similar to the high temperature conditions, through a special sintering process, even texture, density, hardness, compression, flexural, impact resistance and other performance is better than natural stone, durability, to be easily damaged, and no fine cracks common natural stone. Stone is a ceramic stone products, which is based on natural marble, shell, glass, mosaic as the main raw materials, coupled with high-quality polymers as binder, through advanced manufacturing process from refining the green building materials . The stone in the process, through the precise screening, almost completely removed the stone contained radioactive materials, coupled with high performance through high-pressure after the adhesive binder, but it aims to greatly increased degree, some of the intensity even higher than natural stone. Concentrated in the ingredients used in the synthesis process, completely solved the problem of natural stone without support in the renovation process to solve the color problem, especially for the large area of pavement engineering. Natural marble in the process, due to restrictions on the stone itself, the customer only with the size of sheet metal processing, and can not be with their own design. The stone plate size, and have a 3050 × 1250 × 12mm ultra-thin slab, and this is natural stone can not be compared with. The production process is: ore → → broken into different size gravel to join the special stone materials mixing formula → → → vacuum fabric forming a high-side village of diamond gang saw cutting → → → Calibrating wool board, and thickness of thin → vertical and horizontal cutting machine grinding polishing → product → Construction, it should pay attention to include
1. Stone in the transportation, handling process, to avoid rolling fall, collision or injury caused by plate dark crack; outdoor piles should be covered with tarps to rain, wet snow.
2. Installation of cement mortar can not be too wet, too wet cement mortar can cause two problems:
(1) may have a layer of water vapor film, resulting in stone can not be firmly bonded with cement sand;
(2) is difficult to evaporate moisture in the sheet below, to continue with the occurrence of alkali cement the Slate of lead sheet erosion that Qiaojiao even burst.
3. Cement mortar must be mixed evenly, uneven mixing mortar itself ill-structured, in addition to poor adhesion, the case load may occur when the bump.